G Types - Sulfur - Modifies Groups
Grade Mooney Viscosity
[ ML 1+4, 100 ° C ]
Crystallization
Rate
Other Characteristics
GS 40 - 50 Slightly Slow Non-staining, sulfur modified basic G type with best tear strength and flex resistance
GRT 40 - 54 Slow Good low temperature properties G type with best tack for frictioning application
SND16 32 - 39 Slow Lower viscosity version of GRT
GW 37 - 49 Slow Sulfur modified G type with better heat and compression set resistance than GS and GRT
SND46 45 - 60 Slow More peptizable when milled for sponge products
Setüstü Mah.Kabataş Çıkmazı.Saadet Apt. K: 6/12 Kabataş/Beyoğlu/İST
Tel:0212 249 32 15(pbx) Fax:0212 249 31 89